India accelerates defence indigenisation: HAL places Rs 600 crore superalloy order with MIDHANI
- Posted on July 15, 2025
- By Financial Express
- 1 Views

India accelerates defence indigenisation: HAL places Rs 600 crore superalloy order with MIDHANI

HAL has placed a Rs 600 crore order with MIDHANI for advanced superalloys, marking a major step in India’s push for defence indigenisation.